Home » Steel Pipe Fittings » Butt Weld Pipe Fittings » ASTM SB 366 Alloy 400 Monel 400 UNS N04400 Tube bending with excellent resistance to stress corrosion cracking in most freshwaters

ASTM SB 366 Alloy 400 Monel 400 UNS N04400 Tube bending with excellent resistance to stress corrosion cracking in most freshwaters

Monel 400 is widely used in Feed water and steam generator tubing.

Rated 4.5/5 based on 516 customer reviews
Share:
Content

Monel 400 is a nickel-copper alloy that is hardened by cold working only. Monel 400? has low corrosion rate in flowing seawater, therefore it is widely used in marine applications. Monel 400? also has excellent resistance to stress corrosion cracking in most freshwaters. Monel 400 can be used in temperatures up to 1000 ?F. The alloy has great mechanical properties at subzero temperatures.