2205 has excellent corrosion properties, and it is well-suited to environments containing chlorides and hydrogen sulphide, for use in oil and gas extraction from sour wells, in refineries and in process solutions contaminated with chlorides.

Rated 4.9/5 based on 376 customer reviews
Share:
Content

The Duplex steel grade possesses twice the strength of most austenitic and stainless steel grades. This steel has comparably more corrosion resistance than most other grades.

It also has good erosion fatigue properties as well as lower thermal expansion and higher thermal conductivity than austenitic steels. The yield strength is about twice that of austenitic stainless steels, allowing a designer to save weight and make the alloy more cost-competitive when compared to Alloy 316L or Alloy 317L.