Super Duplex 2507 nut with exceptional resistance to chloride stress corrosion cracking

2507 has Combination of properties given by austenitic and ferritic structure, and Good weldability and workability.

Rated 4.7/5 based on 447 customer reviews
Share:
Content

Super Duplex 25 Chrome may experience embrittlement if exposed to temperatures exceeding 480¡ãF (249¡ãC) for extended periods. Also found in Super Duplex are trace amounts of carbon, phosphorus, sulfur, silicon, nitrogen, and copper. Benefits include: good weldability and workability, a high level of thermal conductivity and low coefficient of thermal expansion, high resistance to corrosion, fatigue, high resistance to pitting and crevice corrosion, high resistance to stress corrosion cracking (especially chloride stress corrosion cracking), high energy absorption, high strength, and erosion.