Element
|
310S
|
Carbon
|
0.08
|
Chromium
|
24.0-26.0
|
Nickel
|
19.0-22.0
|
Manganese
|
2.00
|
Silicon
|
1.50
|
Phosphorus
|
0.045
|
Sulfur
|
0.030
|
* Maximum, unless range is indicated
Mechanical Properties
Property
|
310S
|
Yield Strength, min. (ksi)
|
30
|
Tensile Strength, min. (ksi)
|
75
|
Elongation, min. (%)
|
40
|
Hardness, max. (Rb)
|
95
|
Physical Properties
Physical properties for Type 310S stainless steel
Property
|
310S
|
Density, lb/in3
|
0.290
|
Modulus of Elasticity, psi
|
29.0 x 106
|
Coefficient of Thermal Expansion, 68-212˚F, /˚F
|
8.8 x 10-6
|
Thermal Conductivity, Btu/ft hr ˚F
|
8.0
|
Specific Heat, Btu/lb ˚F
|
0.12
|
Electrical Resistivity, Microohm-in
|
30.7
|